B300 spool mild steel MIG wire Oerlikon

Diameters / Packaging

Diameters
15 KG SPOOL (BS300)
1.2 mm W000283171

NIFIL 625

MIG (GMAW)

CLASSIFICATIONS:
AWS A5.14 : ERNiCrMo-3
EN ISO 18274-A : S Ni 6625 (NiCr22Mo9Nb)

Solid wire for welding 9%Ni steels

DETAILS

Used for welding of highly corrosion-resistant Cr-Mo-Nickel base alloys such as alloy 625, alloy 825 and similar alloys. Also suitable for molybdenum alloyed corrosion-resistant steels with e.g. 7% Mo and cold-tough nickel steels

Features

  • In sulphur-free atmospheres the weld metal is non-scaling <1200°C, in sulphurous atmospheres the weld metal can be used <500°C.
  • Used for joining ferritic to austenitic steels (dissimilar) with operating temperatures or postweld heat treatment >300°C.
  • Very resistant to stress corrosion cracking and pitting corrosion in a range of media including phosphoric acid, organic acids, sea water and polluting environments

Typical Applications

  • Cryogenic Applications
  • Cladding
  • Petrochemical
  • Pipelaying
  • LNG

Shielding Gas

  • I1 : Inert gas Ar (100%), I3 : Inert gas Ar+ 0.5-95% He

Service Information