Diameters / Packaging
Diameters |
50 lb Plastic Bag |
---|---|
Flux | ED032990 |
DETAILS
Features
- Neutral submerged arc welding flux designed to meet the specific requirements of wind tower welding applications
- Recommended for use with Lincolnweld L-61 electrode on both longitudinal and circumferential seam welds
- Capable of producing weld deposits with impact properties exceeding 27 J (20 ft lbf) at -62 C (-80 F)
- Smooth bead profile to achieve excellent toe angles, tie-in, and bead appearance on interior and exterior applications
- Actual (Type 3.1) certificates for each lot of flux showing chemical composition, particle size and moisture level are available in the certificate center of lincolnwelectric.com
- Mild Steel Lincolnweld® L-61® Low Alloy Steel Lincolnweld® L-70
Typical Applications
- Wind tower base
- Wind tower door frame
Special Features
- Basicity Index: 1.4 Density: 1.2 g/cm3
Service Information
Documentation
You May Also Need
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
MECHANICAL PROPERTIES
Wire | Classification | Postweld Heat Treatment |
Yield Strength @ 0.2% Offset
MPa (ksi) |
Tensile Strength
MPa (ksi) |
Elongation
% |
Charpy V-Notch
J (ft-lbs) @ -40°C (-40°F) |
Charpy V-Notch
J (ft-lbs) @ -50°C (-60°F) |
Charpy V-Notch
J (ft-lbs) @ -62°C (-80°F) |
---|---|---|---|---|---|---|---|---|
Lincolnweld® L-50® | F7A6-EM13K | As-welded | 500 (73) | 590 (86) | 29 | 89 (66) | ||
Lincolnweld® L-56® | F9A6-EH11K-G | As-welded | 600 (87) | 700 (101) | 26 | 66 (49) | ||
Lincolnweld® L-61® | F6P8-EM12K-H8 | 1 hour @ 620°C (1150°F) | 360 (52) | 460 (67) | 36 | 213 (157) | ||
Lincolnweld® L-61® | F7A8-EM12K-H8 | As-welded | 410 (60) | 520 (75) | 31 | 88 (65) | ||
Lincolnweld® L-70 | F8A4-EA1-A3-H8 | As-welded | 530 (77) | 610 (88) | 26 | 64 (47) | ||
Lincolnweld® LA-71 | F7A6-EM14K-H8 | As-welded | 550 (80) | 630 (91) | 27 | 138 (102) | ||
Lincolnweld® LA-75 | F7A4-ENi1K-G-H8 | As-welded | 500 (72) | 590 (86) | 29 | 144 (106) |
DEPOSIT COMPOSITION
Wire | Classification | %C | %Cr | %Cu | %Mn | %Mo | %Ni | %P | %S | %Si | %Ti |
Diffusible Hydrogen
mL/100g Weld Metal |
---|---|---|---|---|---|---|---|---|---|---|---|---|
Lincolnweld® L-50® | F7A6-EM13K | 0.05 | 0.08 | 2.12 | 0.015 | 0.004 | 0.45 | |||||
Lincolnweld® L-56® | F9A6-EH11K-G | 0.05 | 0.05 | 0.08 | 2.47 | 0.01 | 0.03 | 0.014 | 0.003 | 0.76 | ||
Lincolnweld® L-61® | F6P8-EM12K-H8 | 0.06 | 0.11 | 1.57 | 0.014 | 0.008 | 0.25 | 5 | ||||
Lincolnweld® L-61® | F7A8-EM12K-H8 | 0.06 | 0.07 | 1.72 | 0.012 | 0.008 | 0.32 | 4 | ||||
Lincolnweld® L-70 | F8A4-EA1-A3-H8 | 0.05 | 0.08 | 1.55 | 0.52 | 0.011 | 0.009 | 0.23 | 5 | |||
Lincolnweld® LA-71 | F7A6-EM14K-H8 | 0.06 | 0.08 | 2.00 | 0.012 | 0.005 | 0.62 | 0.02 | 5 | |||
Lincolnweld® LA-75 | F7A4-ENi1K-G-H8 | 0.06 | 0.03 | 0.10 | 1.93 | 0.00 | 0.86 | 0.012 | 0.006 | 0.46 | 5 |
FLUX COMPOSITION
Classification | %Al2O3 | %CaF2 | %CaO | %FeO | %K2O | %MgO | %MnO | %Na2O | %SiO2 | %TiO2 | %ZrO2 |
---|---|---|---|---|---|---|---|---|---|---|---|
Typical Result | 24 | 13 | 4 | 3 | 1 | 23 | 8 | 2 | 18 | 2 | 2 |