Średnica / Opakowanie
Średnice |
Szpula 15 KG |
---|---|
1.2 mm | SC317LP-12 |
Wprowadzenie
SUPERCORE™ 317LP provides improved resistance to pitting in high chloride environments on 317 and 317L stainless steel base metals.
Zalety
- Used to weld 317/317L stainless steels
- Improved resistance to pitting in high chloride environments
- Food processing
Zastosowania standardowe
- Marine
- Chemical process
- Papermaking
- Food processing
Pozycja spawania
- All
Gaz osłonowy
- 80% Argon / 20% CO₂ or 100% CO₂