DETAILS
LINCOLN® ER317/317L has a low carbon content which reduces the possibility of intergranular carbide precipitation - increasing the resistance to intergranular corrosion.
Features
- Weld deposit similar to 316L with a high molybdenum content for increased corrosion resistance
- Ink jet printing identification on entire length of electrode
- Q2 Lot® - Certificate showing actual wire composition and calculated ferrite number (FN) available online
Disclaimers
Service Information
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.9 | ER317, ER317L |
WIRE COMPOSITION
Classification | %C | %Cr | %Cu | %Mn | %Mo | %N | %Nb | %Ni | %P | %S | %Si | Ferrite Number (Delong ©) | Ferrite Number (WRC-1992 ©) |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
ER317 Requirement | 0.08 max. | 18.5 - 20.5 | 0.75 max. | 1.0 - 2.5 | 3.0 - 4.0 | Info. Only | Info. Only | 13.0 - 15.0 | 0.03 max. | 0.03 max. | 0.30 - 0.65 | Info. Only | Info. Only |
ER317L Requirement | 0.03 max. | 18.5 - 20.5 | 0.75 max. | 1.0 - 2.5 | 3.0 - 4.0 | Info. Only | Info. Only | 13.0 - 15.0 | 0.03 max. | 0.03 max. | 0.30 - 0.65 | Info. Only | Info. Only |
Typical Result | 0.01-0.02 | 18.9-19.2 | 0.09-0.12 | 1.4 | 3.5-3.6 | 0.03-0.05 | 0.01 max. | 13.3-13.8 | 0.02 | 0.01 | 0.42-0.50 | 9-15 | 7-12 |