Ultracore stainless, flux-cored wire, plastic spool

Diameters / Packaging

Diameters
10 lb Spool
25 lb Spool
0.047 in (1.2 mm) ED033745 ED033746

Pipeliner® 111M Flux-cored (FCAW-G) Wire

Flux-Cored Gas-Shielded (FCAW-G) | ED033746

CLASSIFICATIONS:
E111T1-GM
E111T1-M21-A4-G

Pipeliner® 111M from Lincoln Electric is designed for hot, fill and cap pass welding on X80 to X100 grade pipe.

DETAILS

A gas-shielded, flux-cored wire designed for hot, fill and cap pass welding of X80 to X100 grade pipe.

Features

  • Consistent Arc – designed for optimal performance in automated pipe welding applications where a consistent

Service Information

BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page

See test result disclaimer

CONFORMANCE

CONFORMANCES SPECIFICATION CLASSIFICATION
AWS AWS A5.29 E111T1-GM
AWS AWS A5.36 E111T1-M21-A4-G

MECHANICAL PROPERTIES

Classification Shielding Gas Polarity Yield Strength @ 0.2% Offset
MPa (ksi)
Tensile Strength
MPa (ksi)
Elongation
%
Charpy V-Notch
J (ft-lbs) @ -20°C (0°F)
Charpy V-Notch
J (ft-lbs) @ -40°C (-40°F)
Hardness Rockwell B Hardness Rockwell C
E111T1-GM Requirement 75-80% Ar, balance CO2 DC+ 680 (98) min. 760-900 (110-130) 15 min. Info. Only
E111T1-M21-A4-G Requirement M21-ArC DC+ 680 (98) min. 760-900 (110-130) 15 min. 27 (20) min. Info. Only
Typical Result, As-welded 75% Ar, 25% CO2 DC+ 690-840 (100-121) 790-880 (114-128) 15-22 76-90 (56-66) 56-78 (41-57) 101-104 22-25

DEPOSIT COMPOSITION

Classification Shielding Gas Polarity %Al %B %C %Cr %Cu %Mn %Mo %Ni %P %S %Si %V Diffusible Hydrogen
mL/100g Weld Metal
E111T1-GM Requirement 75-80% Ar, balance CO2 DC+ Info. Only 0.30 min. * 0.50 min. * 0.20 min. * 0.50 min. * 0.030 max. 0.030 max. 1.00 max. 0.10 min. *
E111T1-M21-A4-G Requirement M21-ArC DC+ 0.18 max.
Typical Result 75% Ar, 25% CO2 DC+ 0.0 max. 0.0047-0.0070 0.07-0.08 0.02-0.06 0.03-0.06 1.45-1.67 0.66-0.79 2.03-2.38 0.007-0.013 0.006-0.009 0.27-0.32 0.01 4

TYPICAL OPERATING PROCEDURES

Diameter Shielding Gas Polarity CTWD
mm (in.)
Wire Feed Speed
m/min (in/min)
Voltage
volts
Approx. Current
amps
Melt-off Rate
kg/hr (lb/hr)
1.2 mm (0.047 in) 75-85% Ar / balance CO2 DC+ 19 (3/4) 4.4-10.2 (175 - 400) 23-30 130 - 275 1.8-4.1 (3.9-9.0)

NOTES

Note
* To meet the requirements of a "G" classification, the chemical composition of the weld deposit must meet the minimum requirement for one or more of these elements.