Techalloy® offers a wide variety of nickel alloy grades of MIG, TIG, and SAW welding products lot tested with certificates of actual wire chemistry and typical mechanical results available online
Features
- This alloy can be age hardened to higher strengths
- Used for welding alloys 718, 706 and X-751
- Mainly used for welding high strength aircraft components and liquid rocket components involving cryogenic temperatures
- Q2 Lot® - Certificate showing actual wire composition available online
Service Information
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.14 | ERNiFeCr-2 |
CWB | AWS A5.14 | ERNiFeCr-2 |
WIRE COMPOSITION
Classification | %Al | %B | %C | %Cr | %Cu | %Fe | %Mn | %Mo | %P | %S | %Si | %Ti | %Nb+Ta | %Ni+Co |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
ERNiFeCr-2 Requirement | 0.20 - 0.80 | 0.006 max. | 0.08 max. | 17.0 - 21.0 | 0.30 max. | Remainder | 0.35 max. | 2.80 - 3.30 | 0.015 max. | 0.015 max. | 0.35 max. | 0.65 - 1.15 | 4.75 - 5.50 | 50.0 - 55.0 |
Typical Result | 0.50 | 0.005 | 0.06 | 17.5 | 0.02 | 20.2 | 0.06 | 3.04 | 0.003 max. | 0.003 max. | 0.04 | 0.93 | 5.11 | 52.5 |
TYPICAL OPERATING PROCEDURES
Diameter | Shielding Gas | Polarity |
Voltage
volts |
Approx. Current
amps |
---|---|---|---|---|
.035" (0.9 mm) | 75% Ar, 25% He | DC+ | 26-29 | 150-190 |
.045" (1.1 mm) | 75% Ar, 25% He | DC+ | 28-32 | 180-220 |
1/16" (1.6 mm) | 75% Ar, 25% He | DC+ | 29-33 | 200-250 |