Diámetros / Embalaje
Diámetros mm |
10 lb (4.5 kg) Plastic Tube |
---|---|
1/8 in (3.2 mm) | TG55125638 |
Detalles
TECHALLOY® 55 weld deposit has a moderate hardness and required carbide tipped tools machineability, preheat and interpass temperature is required on cast iron to minimize the potential for cracks during welding.
Características
- The welds are moderately hard and require carbide tipped tools for machining
- A preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks
- Q2 Lot® - certificates showing actual wire composition available online
Servicio de información
ANTES DE USARLO, LEA Y COMPRENDA LA HOJA DE DATOS DE SEGURIDAD (SDS) DE ESTE PRODUCTO Y LA INFORMACIÓN ESPECÍFICA IMPRESA EN EL ENVASE DEL PRODUCTO. Página de Búsqueda SDS
Ver los resultados de la prueba de limitación de responsabilidad
WIRE COMPOSITION
Classification | %C | %Cu | %Mn | %Ni | %S | %Si | %Al | %Fe |
---|---|---|---|---|---|---|---|---|
Typical Result | 0.0 | 0.1 | 0.7 | 54.0 | 0.0 | 0.1 | 0.1 | 44.5 |