TECH-ROD® 117 provides optimum strength and oxidation resistance between 1500°F to 2100°F, especially when welding on base metals of nickel-iron-chromium alloys.
Características
- A covered electrode used for welding of nickel-chromium-cobalt-molybdenum alloys
- The deposited weld metal provides optimum strength and oxidation resistance between 1500°F to 2100°F, especially when welding on base metals of nickel-iron-chromium alloys
- Q2 Lot® - certificates showing actual deposit composition available online
Servicio de información
ANTES DE USARLO, LEA Y COMPRENDA LA HOJA DE DATOS DE SEGURIDAD (SDS) DE ESTE PRODUCTO Y LA INFORMACIÓN ESPECÍFICA IMPRESA EN EL ENVASE DEL PRODUCTO. Página de Búsqueda SDS
Ver los resultados de la prueba de limitación de responsabilidad
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.11 | ENiCrCoMo-1 |
MECHANICAL PROPERTIES
Classification |
Tensile Strength
MPa (ksi) |
Elongation
% |
---|---|---|
ENiCrCoMo-1 Requirement | 620 (90) min. | 25 min. |
Typical Result, As-welded | 770 (112) | 40 |
DEPOSIT COMPOSITION
Classification | %C | %Co | %Cr | %Cu | %Fe | %Mn | %Mo | %Ni | %P | %S | %Si | %Nb+Ta |
---|---|---|---|---|---|---|---|---|---|---|---|---|
ENiCrCoMo-1 Requirement | 0.05 - 0.15 | 9.0 - 15.0 | 21.0 - 26.0 | 0.50 max. | 5.0 max. | 0.3 - 2.5 | 8.0 - 10.0 | Remainder | 0.03 max. | 0.015 max. | 0.75 max. | 1.0 max. |
Typical Result | 0.11 | 11.4 | 24.8 | 0.01 | 0.9 | 1.1 | 9.3 | 51 | 0.02 | 0.005 | 0.44 | 0.9 |
TYPICAL OPERATING PROCEDURES
Diameter |
Current
Amps |
---|---|
3/32" (2.4 mm) | 65-85 |
1/8" (3.2 mm) | 80-110 |
5/32" (4.0 mm) | 100-140 |
3/16" (4.8 mm) | 110-160 |