Détails
- Grinox® 10 features good resistance to intergranular corrosion up to
400°C and good resistance to pitting corrosion into enviornments containing non-oxidizing acids - Good resistance to scaling in presence of air and oxidizing combustion gases up to 800°C
Traits
- No escama en presencia de aire y gases oxidantes de combustión hasta temperaturas de 800°C.
- Posiciones de soldadura: todas, excepto vertical descendent
- Fabricación de tanques, tuberías y equipos para las industrias: química, alimenticia, textil y farmacéutica.
Disclaimers
Des informations de service
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.4 | E316L-16 |
MECHANICAL PROPERTIES
Classification |
Tensile Strength
MPa (ksi) |
Elongation
% |
---|---|---|
E316L-16 Requirement | 480 (70) min. | 30 min. |
Typical Result, As-welded | 564 (82) | 49 |
DEPOSIT COMPOSITION
Classification | %C | %Cr | %Cu | %Mn | %Mo | %N | %Ni | %P | %S | %Si | Ferrite Number (WRC-1992 ©) |
---|---|---|---|---|---|---|---|---|---|---|---|
E316L-16 Requirement | 0.04 max. | 17.0 - 20.0 | 0.75 max. | 0.5 - 2.5 | 2.0 - 3.0 | Info. Only | 11.0 - 14.0 | 0.04 max. | 0.03 max. | 1.00 max. | Info. Only |
Typical Result | 0.03 | 18.0 | 0.12 | 0.8 | 2.5 | 0.05 | 11.5 | 0.03 | 0.02 | 0.60 | 4-9 |
TYPICAL OPERATING PROCEDURES
Diameter | Polarity⁽¹⁾ |
Current
Amps |
---|---|---|
3/32" (2.4 mm) | AC | 70-85 |
1/8" (3.2 mm) | AC | 85-110 |
5/32" (4.0 mm) | AC | 110-140 |
3/32" (2.4 mm) | DC+ | 70-85 |
1/8" (3.2 mm) | DC+ | 85-110 |
5/32" (4.0 mm) | DC+ | 110-140 |
NOTES
Note |
---|
⁽¹⁾ Suggested polarity is listed first |