2.4 mm | T9CRMO-24 |
DETTAGLI
Bacchetta TIG per lega martensitica al 9%Cr-1%Mo per il servizio a temperature elevate fino a 600°C
Caratteristiche
- B8 alloyed steel: 9% chromium, 1% molybdenum martensitic alloy for elevated temperature service up to 600°C (1112°F)
- Designed for high strength and improved corrosion resistance in superheated steam, hot hydrogen gas and high sulphur crude oils where higher performance than 5% chromium, 0.5% molybdenum steels is required
- Disponibile in un tubo in PE
Informazioni sui servizi
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. Pagina di ricerca SDS
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.28 | ER80S-B8 |
MECHANICAL PROPERTIES
Classification | Postweld Heat Treatment | Shielding Gas | Polarity |
Yield Strength @ 0.2% Offset
MPa (ksi) |
Tensile Strength
MPa (ksi) |
Elongation
% |
---|---|---|---|---|---|---|
ER80S-B8 Requirement | 100% Ar | DC- | 470 (68) min. | 550 (80) min. | 17 min. | |
Typical Result, Stress relieved | 1 hour @ 745°C (1375°F) | 100% Ar | DC- | 600 (88) | 720 (104) | 23 |
WIRE COMPOSITION
Classification | %C | %Cr | %Mn | %Mo | %Ni | %P | %S | %Si | %Total Cu |
---|---|---|---|---|---|---|---|---|---|
ER80S-B8 Requirement | 0.10 max. | 8.00 - 10.50 | 0.40 - 0.70 | 0.80 - 1.20 | 0.50 max. | 0.025 max. | 0.025 max. | 0.50 max. | 0.35 max. |
Typical Result | 0.09 | 8.58 | 0.51 | 0.94 | 0.08 | 0.016 | 0.002 | 0.42 | 0.05 |