DETAILS
Stainless steel welding rods designed to provide optimal bead appearance when TIG welding on a variety of materials
Features
- Used to overlay mild and low alloy steels
- Preheat and inter-pass temperatures of 300°F (150°C) or greater are recommended during welding
- Post-weld heat treatment should not exceed 1150°F (620°C) as higher temperatures may result in hardening
Typical Applications
- Process Piping
- Chemical processing
- Power Generation
Welding Positions
- All
Shielding Gas
- 100% Argon
Disclaimers
Service Information
Documentation
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.9 | ER410NiMo |
WIRE COMPOSITION
Classification | %C | %Cr | %Cu | %Mn | %Mo | %N | %Nb | %Ni | %P | %S | %Si |
---|---|---|---|---|---|---|---|---|---|---|---|
ER410NiMo Requirement | 0.06 max. | 11.0 - 12.5 | 0.75 max. | 0.6 max. | 0.4 - 0.7 | Info. Only | Info. Only | 4.0 - 5.0 | 0.03 max. | 0.03 max. | 0.5 max. |
Typical Result | 0.02-0.03 | 11.8-12.1 | 0.04-0.06 | 0.4-0.5 | 0.5-0.6 | 0.02-0.05 | 0.00 max. | 4.5-4.7 | 0.01-0.02 | 0.01 max. | 0.4 |