Detalles
LINCOLN® ER2594 electrode is over-alloyed with nitrogen to provide the optimum ferrite/austenite ratio in the finished weld resulting in high tensile and yield strength and superior resistance to stress corrosion, cracking (SCC) and pitting corrosion.
Características
- A super-duplex grade electrode that provides matching chemistry and mechanical property characteristics to wrought super duplex alloys such as 2507 and Zeron 100, as well as to super-duplex casting alloys (ATSM A890)
- The electrode is over-alloyed with nitrogen to provide the optimum ferrite/austenite ratio in the finished weld resulting in high tensile and yield strength and superior resistance to stress corrosion, cracking (SCC) and pitting corrosion
- Ink jet printing identification on entire length of electrode
- Q2 Lot® - Certificate showing actual wire composition and calculated ferrite number (FN) available online
Servicio de información
ANTES DE USARLO, LEA Y COMPRENDA LA HOJA DE DATOS DE SEGURIDAD (SDS) DE ESTE PRODUCTO Y LA INFORMACIÓN ESPECÍFICA IMPRESA EN EL ENVASE DEL PRODUCTO. Página de Búsqueda SDS
Ver los resultados de la prueba de limitación de responsabilidad
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.9 | ER2594 |
ABS | AWS A5.9 | ER2594 |
WIRE COMPOSITION
Classification | %C | %Cr | %Cu | %Mn | %Mo | %N | %Ni | %P | %S | %Si | %W | Ferrite Number (Delong ©) | Ferrite Number (WRC-1992 ©) |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
ER2594 Requirement | 0.03 max. | 24.0 - 27.0 | 1.5 max. | 2.5 max. | 2.5 - 4.5 | 0.20 - 0.30 | 8.0 - 10.5 | 0.03 max. | 0.02 max. | 1.0 max. | 1.0 max. | ||
Typical Result | 0.01-0.02 | 24.8-25.2 | 0.1 | 0.6 | 3.9-4.0 | 0.24-0.26 | 8.6-9.1 | 0.02 | 0.003 max. | 0.4 | 0.0 max. | 28 | 45-50 |