Detalles
LINCOLN® ER308/308L provides a balanced chromium and nickel levels provide enough ferrite in the weld for high resistance to hot cracking, dual classification ensures the maximum carbon content is 0.03% and ink jet printing identification on entire length of electrode.
Características
- Balanced chromium and nickel levels provide enough ferrite in the weld for high resistance to hot cracking
- Dual classification ensures the maximum carbon content is 0.03%
- 0.03% carbon content increases resistance to intergranular corrosion
- Ink jet printing identification on entire length of electrode
- Q2 Lot® - Certificate showing actual wire composition and calculated ferrite number (FN) available online
Servicio de información
También puede necesitar
ANTES DE USARLO, LEA Y COMPRENDA LA HOJA DE DATOS DE SEGURIDAD (SDS) DE ESTE PRODUCTO Y LA INFORMACIÓN ESPECÍFICA IMPRESA EN EL ENVASE DEL PRODUCTO. Página de Búsqueda SDS
Ver los resultados de la prueba de limitación de responsabilidad
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.9 | ER308, ER308L |
ABS | AWS A5.9 | ER308, ER308L |
CWB | CSA W48 | ER308, ER308L |
MIL | MIL-E-19933E AMD1 | MIL-308, MIL-308L |
WIRE COMPOSITION
Classification | %C | %Cr | %Cu | %Mn | %Mo | %N | %Nb | %Ni | %P | %S | %Si | %Ti | Ferrite Number (Delong ©) | Ferrite Number (WRC-1992 ©) |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
ER308 Requirement | 0.08 max. | 19.5 - 22.0 | 0.75 max. | 1.0 - 2.5 | 0.75 max. | 9.0 - 11.0 | 0.03 max. | 0.03 max. | 0.30 - 0.65 | |||||
ER308L Requirement | 0.03 max. | 19.5 - 22.0 | 0.75 max. | 1.0 - 2.5 | 0.75 max. | 9.0 - 11.0 | 0.03 max. | 0.03 max. | 0.30 - 0.65 | |||||
Typical Result | 0.01-0.02 | 19.7-20.3 | 0.04-0.33 | 1.2-1.9 | 0.06-0.15 | 0.02-0.06 | 0.02 max. | 10.1-10.4 | 0.02 | 0.01 max. | 0.34-0.57 | 0.00 max. | 10-16 | 10-14 |