UltraCore flux-cored wire
UltraCore flux-cored wire

Diámetros / Embalaje

Diámetros
mm
33 lb Spool
1/16 in (1.6 mm) ED037121

UltraCore® FC 309L

Soldadura con Núcleo de Fundente Protegido con Gas (FCAW-G) | ED037121

CLASIFICACIONES:
E309LT0-1
E309LT0-4

UltraCore FC 308L está diseñado para soldaduras de todas posiciones, brinda un desempeño superior de soldadura y manejo mejorado para el operador

Detalles

ULTRACORE® 309L provides polished weld bead appearance, smooth arc action with minimal spatter reduces post-weld cleaning and delivers steady consistent wire feeding during welding operations.

Características

  • Precision layer wound winding delivers steady spool payoff and more consistent feeding
  • Smooth arc action with minimal spatter reduces post-weld cleaning
  • Polished weld bead appearance reduces post-weld brushing

Servicio de información

También puede necesitar

ANTES DE USARLO, LEA Y COMPRENDA LA HOJA DE DATOS DE SEGURIDAD (SDS) DE ESTE PRODUCTO Y LA INFORMACIÓN ESPECÍFICA IMPRESA EN EL ENVASE DEL PRODUCTO. Página de Búsqueda SDS

Ver los resultados de la prueba de limitación de responsabilidad

CONFORMANCE

CONFORMANCES SPECIFICATION CLASSIFICATION
AWS AWS A5.22 E309LT0-1, E309LT0-4
ABS AWS A5.22 E309LT0-1, E309LT0-4
CWB AWS A5.22 E309LT0-1, E309LT0-4

MECHANICAL PROPERTIES

Classification Shielding Gas Tensile Strength
MPa (ksi)
Elongation
%
Longitudinal Face Bend
E309LT0-1 Requirement 100% CO2 520 (75) min. 30 min. No opening in excess of 1/8 inch
E309LT0-4 Requirement 75-80% Ar, balance CO2 520 (75) min. 30 min. No opening in excess of 1/8 inch
Typical Result, As-welded 100% CO2 580 (84) 36 Passed
Typical Result, As-welded 75% Ar, 25% CO2 540 (79) 42 Passed

DEPOSIT COMPOSITION

Classification Shielding Gas %C %Cr %Cu %Mn %Mo %N %Ni %P %S %Si Ferrite Number (per AWS A4.2)
E309LT0-1 Requirement 100% CO2 0.04 max. 22.0 - 25.0 0.75 max. 0.5 - 2.5 0.75 max. Info. Only 12.0 - 14.0 0.04 max. 0.03 max. 1.0 max. Info. Only
E309LT0-4 Requirement 75-80% Ar, balance CO2 0.04 max. 22.0 - 25.0 0.75 max. 0.5 - 2.5 0.75 max. Info. Only 12.0 - 14.0 0.04 max. 0.03 max. 1.0 max. Info. Only
Typical Result 100% CO2 0.04 23.9 0.07 1.4 0.15 0.04 12.6 0.02 0.01 0.7 19
Typical Result 75% Ar, 25% CO2 0.04 23.8 0.07 1.3 0.15 0.04 12.7 0.02 0.01 0.7 19

TYPICAL OPERATING PROCEDURES

Diameter Shielding Gas Polarity CTWD
mm (in.)⁽¹⁾
Wire Feed Speed
m/min (in/min)
Voltage
volts
Approx. Current
amps
Melt-off Rate
kg/hr (lb/hr)
Deposition Rate
kg/hr (lb/hr)
Efficiency
%
0.045 in (1.1 mm) 75% Ar / 25% CO2 DC+ 19 (3/4) 5.3 (210) 22-24 140 2.1 (4.6) 1.9 (4.2) 91.3
0.045 in (1.1 mm) 75% Ar / 25% CO2 DC+ 19 (3/4) 8.9 (350) 24-26 185 3.9 (8.7) 3.4 (7.5) 86.2
0.045 in (1.1 mm) 75% Ar / 25% CO2 DC+ 19 (3/4) 11.4 (450) 26-28 225 4.7 (10.3) 4.4 (9.6) 93.2
1/16 in (1.6 mm) 75% Ar / 25% CO2 DC+ 25 (1) 3.6 (140) 23-25 165 2.7 (5.9) 2.3 (5.0) 84.7
1/16 in (1.6 mm) 75% Ar / 25% CO2 DC+ 25 (1) 6.4 (250) 25-27 235 4.8 (10.6) 4.2 (9.3) 87.7
1/16 in (1.6 mm) 75% Ar / 25% CO2 DC+ 25 (1) 8.1 (320) 26-28 290 6.1 (13.5) 5.4 (12) 88.8

NOTES

Note
⁽¹⁾ To estimate ESO, subtract 1/4 in. (6.0 mm) from CTWD.