Diameters / Packaging
Diameters |
2 LB SPOOL |
10 LB SPOOL |
---|---|---|
0.035 IN | ED034465 | ED034469 |
0.045 IN | ED034466 | ED034470 |
DETAILS
Designed for prolonged elevated temperatures up to 550°C (1022°F).
Features
- Ultra clean wire
- X factor &le
- 10 ppm
- Designed for welding 1.25% chromium, 0.50% Molybdenum steels
- Designed for prolonged elevated temperatures up to 550°C (1022°F)
- Capable of exceeding AWS minimum requirement of 550 MPa (80 ksi) tensile strength after 8 hours of stress relieving at 620°C (1150°F)
- Precision Layer Wound
Typical Applications
- Petrochemical
- Power Generation
- Power Plants
- Process Piping
- Turbine Castings
Welding Positions
- All
Shielding Gas
- 100% Argon
Disclaimers
Service Information
Documentation
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.28 | ER80S-B2 |
MECHANICAL PROPERTIES
Classification | Shielding Gas | Polarity |
Yield Strength @ 0.2% Offset
MPa (ksi) |
Tensile Strength
MPa (ksi) |
Elongation
% |
---|---|---|---|---|---|
ER80S-B2 Requirement | 100% Ar | DC- | 470 (68) min. | 550 (80) min. | 19 min. |
Typical Result, 1 hour @ 620°C (1150°F) | 100% Ar | DC- | 580 (84) | 690-750 (100-108) | 26 |
WIRE COMPOSITION
Classification | %C | %Cr | %Mn | %Mo | %Ni | %P | %S | %Si | %Total Cu |
---|---|---|---|---|---|---|---|---|---|
ER80S-B2 Requirement | 0.07 - 0.12 | 1.20 - 1.50 | 0.40 - 0.70 | 0.40 - 0.65 | 0.20 max. | 0.025 max. | 0.025 max. | 0.40 - 0.70 | 0.35 max. |
Typical Result | 0.10-0.11 | 1.33-1.40 | 0.54-0.56 | 0.46-0.52 | 0.03-0.14 | 0.003-0.005 | 0.003-0.004 | 0.54-0.56 | 0.20-0.23 |