DETAILS
SuperGlaze® 5183 Aluminum Magnesium Manganese filler rod is commonly used for higher strength welding of 5XXX and 6XXX base materials. Higher strength and superior salt water corrosion resistance with common shipbuilding base materials compared to 5356.
Features
- Designed for applications where higher strength is required
- Provides very high as-welded strength for high magnesium alloys such as 5083
- Excellent corrosion resistance ideal for shipbuilding and marine applications
- Alloy embossed on each rod for easy identification
Typical Applications
- Shipbuilding
- Pressure vessels
- Cryogenic tanks
Welding Positions
- All except vertical down
Shielding Gas
- 100% Argon Argon / Helium Mixtures Flow Rate: 30 - 50 CFH
Special Features
- Q2 Lot® Certificate - Certified Material Test Report showing actual wire composition
Disclaimers
Service Information
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.10 | ER5183 |
WIRE COMPOSITION
Classification | %Be | %Cr | %Cu | %Fe | %Mg | %Mn | %Si | %Ti | %Zn |
---|---|---|---|---|---|---|---|---|---|
ER5183 Requirement | 0.0003 max. | 0.05 - 0.25 | 0.10 max. | 0.40 max. | 4.3 - 5.2 | 0.50 - 1.0 | 0.40 max. | 0.15 max. | 0.25 max. |
Typical Result | 0.0002 max. | 0.07 | 0.00 | 0.12 | 4.9 | 0.6 | 0.05 | 0.07 | 0.01 |