Techalloy® 55 TIG (GTAW) Wire

TIG (GTAW) | TG55125638

CLASSIFICATIONS:
AWS Similar to ENiFe-Cl

For cast iron joining and repair

DETAILS

TECHALLOY® 55 is ideal for a preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks.

Features

  • The welds are moderately hard and require carbide tipped tools for machining
  • A preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks
  • Q2 Lot® - certificates showing actual wire composition available online

Disclaimers

Warning -

Cancer and Reproductive Harm -

www.P65Warnings.ca.gov

BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page

See test result disclaimer

WIRE COMPOSITION

Classification %C %Cu %Mn %Ni %S %Si %Al %Fe
Typical Result 0.0 0.1 0.7 54.0 0.0 0.1 0.1 44.5