Lincolnweld® LA-85

Soldadura por arco sumergido (SAW) | ED023167

CLASIFICACIONES:
ENi5

Lincolnweld® LA-85 Capaz de producir depósitos de soldadura con resistencia a la tensión de 480-550 MPa (70-80 ksi) en las condiciones de cómo se soldó y de relevado de esfuerzos.

Detalles

  • A nickel-bearing wire with 0.2% molybdenum designed for use on weathering steels
  • Capable of producing weld deposits with 480-550 MPa (70-80 ksi) tensile strength in the as-welded and stress-relieved conditions

Características

  • A nickel-bearing wire with 0.2% molybdenum designed for use on weathering steels
  • Capable of producing weld deposits with 480-550 MPa (70-80 ksi) tensile strength in the as-welded and stress-relieved conditions
  • Actual (Type 3.1) certificates for each lot of wire showing chemical composition are available in the certificate center of lincolnelectric.com